| Cutting Range | Welding Range | Heating Range | |||||||
|---|---|---|---|---|---|---|---|---|---|
| As Is | With Options | As Is | With Options | As Is | With Options | ||||
| Purox Metal Master | To 1-1/2" | To 8 " | To 3/8" | To 1" | To 30 cfh acetylene (44,000 btu/hr) | 200 cfh acetylene (294,000 btu/hr) | |||
| Purox GT-350 | To 1-1/2" | To 8 " | To 3/8" | To 1" | To 30 cfh acetylene (44,000 btu/hr) | 200 cfh acetylene (294,000 btu/hr) | |||
| Oxweld GT-450 | To 1-1/2" | To 8 " | To 1/4" | To 15 cfh acetylene (22,000 btu/hr) | 200 cfh acetylene (294,000 btu/hr) | ||||
| Purox GT-510 | To 1-1/2" | To 8 " | To 1" | To 30 cfh acetylene (44,000 btu/hr) | 200 cfh acetylene (294,000 btu/hr) | ||||
| Oxweld GT-510 | To 1-1/2" | To 8 " | To 1" | To 30 cfh acetylene (44,000 btu/hr) | 200 cfh acetylene (294,000 btu/hr) | ||||
| Purox 300 FlameMaster | To 4" | To 1/8" | 81,000 btu/hr | ||||||
| Oxweld 400 FlameMaster | To 8 " | To 1/8" | 81,000 btu/hr | ||||||
| Purox E Master | To 4" | To 12 " | |||||||